Study on the Fracture Toughness of FCA Weldment with the Yield Strength 420MPa Grade High Strength Steels for Offshore Structures Depending on the Welding Position
In-Chan Kim, Sang-Hoon Jeong, Han-Geul Choi, Myung-Hyun Kim
J Weld Join. 2018;36(2):67-73.   Published online April 2, 2018
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031897
Microstructure and Mechanical Properties of Reheated Zones in the Multi-pass Weld Metal of High-Strength Steel
Yongjoon Kang, Gitae Park, Seonghoon Jeong, Changhee Lee
J Weld Join. 2017;35(6):21-26.   Published online December 21, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031893
A Basic Study on Brittle Crack Propagation Path with Ultra Large Steel Plate Weld Joints
Gyubaek An, Illwook Han, Jeongung Park, Wan Chuck Woo
J Weld Join. 2017;35(6):15-20.   Published online December 8, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Identification of Correlation Between Fracture Toughness Parameters of Cryogenic Steel Weld Joints
Gyubaek An, Seunglae Hong, Jeongung Park, Chanseung Ro, Ilwook Han
J Weld Join. 2017;35(3):82-87.   Published online June 30, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Effect of Post-Weld Heat Treatment on the Mechanical Properties and Microstructure of P-No. 1 Carbon Steels
Seung-Gun Lee, Yongjoon Kang, Gi-Dong Kim, Sung-Sik Kang
J Weld Join. 2017;35(1):26-33.   Published online February 28, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031738
Characteristic and Measurement Technology of Inner Welding Residual Stresses in Thick Steel Structures
Jeong-ung Park, Gyu-baek An, Wanchuck Woo
J Weld Join. 2016;34(2):16-21.   Published online April 30, 2016
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031712
Effect of Groove Conditions on the Mechanical Properties of Welds Produced by the Combined Welding Process of Flux Cored Arc and Electro Gas in EH36 TMCP Steel Plate for Hull Structures
Kihyuk Kim, Kiwon Kim, Hoseop Sim, Kangho Bae, Hyunuk Hong, Byunggyu Park
J Weld Join. 2015;33(5):35-40.   Published online October 30, 2015
PDFPDF    
2031663
Design for avoid unstable fracture in shipbuilding and offshore plant structure
Gyubaek An, Hong-Yeol Bae, Byung-Doo Noh et al.
J Weld Join. 2015;33(1):35-40.   Published online February 28, 2015
PDFPDF    
2031651
Effects of C on the Strength and Toughness of FCAW Weld Metal of YS 460 MPa Steels for Ship and Offshore Structures
Sang-Hoon Jeong, Jeong-Ho Eom, Han-Geul Choi, Byung-Ho Jeong, Sung-Hwa Hur, Chang-Yong Kang
J Weld Join. 2014;32(6):565-570.   Published online December 31, 2014
PDFPDF    
Effects of PWHT on Weld Metal Properties of YS 460 MPa Steels for Ship and Offshore Structures
Chang-Yong Kang, Sang-Hoon Jeong
J Weld Join. 2014;32(4):413-417.   Published online August 30, 2014
PDFPDF    
Effects of PWHT on Tensile Properties and Impact Toughness of FCAW Weld Metal of FH Steels for Cargo Tank in LPG Carrier
Sang-Hoon Jeong, Chang-Yong Kang
J Weld Join. 2014;32(4):401-406.   Published online August 30, 2014
PDFPDF    
2031572
Effect of Heat Input of Outside Weld on Low Temperature Toughness of Inside Weld for Multiple Electrode SA Welded API 5L X70 with Sour Gas Resistance
Hyun-Jun An, Hee-Keun Lee, Young-Gyu Park, Seong-Su Eun, Chung-Yun Kang
J Weld Join. 2014;32(1):93-101.   Published online February 27, 2014
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI